Al6XN 12 X 12 Stainless Steel Plate

Al6XN 12 X 12 Stainless Steel Plate


1.Standard: ASTM A240 / ASME SA240
2.Thickness: 0.1mm-200mm
3.Width: 800-3000mm
4.Length: 1000-6000mm
Wyślij zapytanie
Wprowadzenie produktów

Al6XN 12 x 12 stainless steel plate is known for its exceptional corrosion resistance, particularly in aggressive environments such as chloride-containing solutions, seawater, and acidic conditions. It is composed of a combination of chromium, nickel, molybdenum, and nitrogen, which contributes to its outstanding resistance to pitting corrosion, crevice corrosion, and stress corrosion cracking.

 

ASTM B688 UNS N08367 Stainless Steel Plate Applications:

Al6XN 12 x 12 Stainless Steel Plate

Al6XN 12 x 12 Stainless Steel Plate Chemical Composition

23.5-25.5
20.00-22.00
6.00-7.00
C 0.03 Max
N 0.18-0.25
2.0 Max
1.00 Max
P .040 Max
S 0.03 Max
0.75 Max

 

ASTM B688 UNS N08367 Sheet Mechanical Properties

.2% Yield Strength, psi Elongation in 2", percent Charpy V-Notch Toughness, ft-lb

-450 (-268)

218,000

142,000

36

353*

-320 (-196)

196,000

107,000

49

85

-200 (-129)

-

-

-

100

70 (21)

108,000

53,000

47

140

200 (93)

99,900

49,400

47

-

400 (204)

903,000

40,400

46

-

600 (316)

86,000

36,300

47

-

800 (427)

87,000

36,000

48

-

 

Al6XN Plate High Temperature Resistance

ASTM B688 Al6XN stainless steel plate has excellent high temperature resistance. Typically withstands temperatures ranging from 900 degree (1652 degree F) to 1000 degree (1832 degree F). 

 

12 x 12 Stainless Steel Plate Sizes and Dimensions

The 1/4" or 1/8" thickness provides stability and rigidity, making it ideal for structural and load-bearing purposes. The 12 x 12 Stainless Steel Plate

 

Q: What Is The Alloy al6xn Price?

A: $8-$10 Price Per Kg

A: 7-21days

A: A Mill Test Certificate (Mtc), Or Mill Test Report (Mtr), Also Known As An En 10204 Certificate

 

 

Popularne Tagi: al6xn stainless steel plate, al6xn plate, al6xn stainless steel

Wyślij zapytanie

whatsapp

Telefon

Adres e-mail

Zapytanie